Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a broad range of demanding application requirements. Vydyne extrusion grade resins provide good resistance to a wide variety of chemicals, solvents, gasoline, and machine and motor oils. Vydyne 66B Series resins are of high-molecular-weight grade developed to provide high and controlled melt strength. Vydyne 66J Resins are heat-stabilized version for added resistance to elevated temperature use. The high viscosity of Vydyne 66J allows for a very stable and easily controlled melt extrudate. Vydyne 66B and 66J are recognized by Underwriters Laboratories.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; ISO 62
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm

@Thickness 2.00 mm
0.015 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527
Elongation at Yield 25 %
25 %
ISO 527
Tensile Modulus 1.30 GPa
189 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Processing Properties Metric English Comments
Processing Temperature 250 - 295 °C
482 - 563 °F
Die Temperature 270 - 295 °C
518 - 563 °F
Melt Temperature 270 - 295 °C
518 - 563 °F
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Copyright © lookpolymers.com All Rights Reserved