Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 12 - 18 hour | 12 - 18 hour | Demold time, catalyzed with QM 264B |
ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 264 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |