Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | <= 12 hour | <= 12 hour | |
Entec Hylox® 9020 PBT, 20% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Dry Time | <= 12 hour | <= 12 hour | |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Dry Time | <= 12 hour | <= 12 hour | |
Entec Hylox® 9230BK PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Dry Time | <= 12 hour | <= 12 hour | |
Entec Hylox® 9015 PBT, 15% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Dry Time | 12 hour | 12 hour | Light traffic ready |
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Hard |
Abatron MasterMold 12-8 Flexible Mold Making Compound Master mold 12-8 is a pourable version of MasterMold 12-3 for creating a mold by pouring it into, or around, the model.Processing: Part A Resin: Clear, pourable viscous liquid, 8.7 lbs/galPart B Con.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT PURPLE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT PURPLE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT PURPLE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT 135 |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT 140 |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Dry Time | 12 - 18 hour | 12 - 18 hour | Demold time, catalyzed with QM 264B |
ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 264 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Dry Time | 12 - 16 hour | 12 - 16 hour | Demold time, catalyzed with QM CAT PURPLE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |