Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4000TF Polyamide-imide (PAI)
(Unverified Data**) Torlon 4000TF is a neat resin polyamide-imide (PAI) fine powder designed for compounding with other polymers and specialty additives. It is the base resin utilized in all Torlon injection molded com.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Drying Temperature | 177 °C @Time 14400 sec |
351 °F @Time 4.00 hour |
|
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491.. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 4000T Polyamide-imide (PAI) Torlon® 4000T is a neat resin polyamide-imide (PAI) coarse powder designed for compounding with other polymers and specialty additives. It is the base resin utilized in all Torlon injection molde.. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI) Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a .. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Drying Temperature | 177 °C @Time 10800 sec |
351 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Drying Temperature | 177 °C @Time 9000 sec |
351 °F @Time 2.50 hour |
|
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Drying Temperature | 177 °C @Time 9000 sec |
351 °F @Time 2.50 hour |
|
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Drying Temperature | 177 °C @Time 9000 sec |
351 °F @Time 2.50 hour |
|
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Drying Temperature | 177 °C @Time 9000 sec |
351 °F @Time 2.50 hour |
|
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Drying Temperature | 177 °C @Time 9000 sec |
351 °F @Time 2.50 hour |
|
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified) Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Drying Temperature | 177 °C | 351 °F | |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |