Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 105 °C | 158 - 221 °F | Average value: 84.8 °C Grade Count:34 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 87.9 °C Grade Count:4 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 84.7 °C Grade Count:4 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 85.5 °C Grade Count:5 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 86.1 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Drying Temperature | 90.0 - 105 °C @Time 14400 - 21600 sec |
194 - 221 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Drying Temperature | 95.0 - 105 °C | 203 - 221 °F | Injection Molding |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 105 °C @Time 14400 - 21600 sec |
194 - 221 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Drying Temperature | 90.0 - 105 °C @Time 14400 - 21600 sec |
194 - 221 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-451PG Electroplating PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor.. |
|||
Drying Temperature | 90.0 - 105 °C @Time 14400 - 21600 sec |
194 - 221 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Drying Temperature | 90.0 - 105 °C | 194 - 221 °F | |
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 85.0 °C Grade Count:11 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 85.0 °C Grade Count:49 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Drying Temperature | 60.0 - 105 °C | 140 - 221 °F | Average value: 80.0 °C Grade Count:33 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |