Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-113 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-1162 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-117 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-220 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-301 Flame Retardant Polystyrene
Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-960 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier ..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-960PC Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmNon-DPO, UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housingInforma..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-980 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold..
Rear Barrel Temperature 180 - 205 °C
356 - 401 °F
Start Point: 190°C
Kingfa H-12 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa HC-110 Modified ABS
Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa HIPS-5197 High Impact Polystyrene
Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa HP-126 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Rear Barrel Temperature 180 - 205 °C
356 - 401 °F
Start Point: 190°C
Kingfa HR-527 Modified ABS
Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Rear Barrel Temperature 180 - 205 °C
356 - 401 °F
Start Point: 190°C
Kingfa HR-527A Modified ABS
Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Rear Barrel Temperature 185 - 205 °C
365 - 401 °F
Injection Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
Rear Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-100 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-8002 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPS-930 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec..
Rear Barrel Temperature 182 - 205 °C
360 - 401 °F
Start Point: 190°C
Kingfa FRHIPSV-0 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud..
Rear Barrel Temperature 185 - 205 °C
365 - 401 °F
Chi Mei Acryrex® CM-205 PMMA
High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather ..