Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TPSF-FR1 PBT, 30% Glass Reinforced Structural Foam Grade, Flame Retardant Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Mold Temperature | 60.0 - 87.8 °C | 140 - 190 °F | |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 60.0 - 87.8 °C | 140 - 190 °F | |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (Cond) Information provided by Ravago. |
|||
Mold Temperature | 60.0 - 87.8 °C | 140 - 190 °F | |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BU00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled
(Unverified Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 66.0 - 88.0 °C | 151 - 190 °F | |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |