Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |