Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 282 - 310 °C | 540 - 590 °F | Average value: 299 °C Grade Count:13 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |