Processing Properties Metric English Comments
Nozzle Temperature 191 - 216 °C
376 - 421 °F
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE)
Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa..
Nozzle Temperature 191 - 216 °C
376 - 421 °F
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE)
Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Nozzle Temperature 191 - 232 °C
375 - 450 °F
Star Plastics ABS450FR Molding Grade ABS
Information provided by Star Plastics, Inc.
Nozzle Temperature 191 - 232 °C
375 - 450 °F
Star Plastics ABSFR1 Molding Grade ABSFR
Information provided by Star Plastics, Inc.
Nozzle Temperature 191 - 232 °C
375 - 450 °F
Star Plastics ABSFR2 Molding Grade ABS
Information provided by Star Plastics, Inc.
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design..
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F..
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design..
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol..
Nozzle Temperature 191 - 235 °C
375 - 455 °F
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 - 210 °C
375 - 410 °F
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 °C
375 °F
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 191 - 229 °C
375 - 445 °F
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Nozzle Temperature 191 °C
376 °F
Typical Die Temp.
DuPont Nucrel® 0903B Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film  (discontinued **)
9 wt% Methacrylic Acid.Nucrel® 0903B is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion processes designed to process polyethylene re..