Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 191 - 216 °C | 376 - 421 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Nozzle Temperature | 191 - 216 °C | 376 - 421 °F | |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Nozzle Temperature | 191 °C | 376 °F | Typical Die Temp. |
DuPont Nucrel® 0903B Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 9 wt% Methacrylic Acid.Nucrel® 0903B is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion processes designed to process polyethylene re.. |