Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM 792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 seconds; ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
Elastic; ASTM D412
4.65 MPa

@Strain 100 %
675 psi

@Strain 100 %
ASTM D412
Elongation at Break 620 %
620 %
Elastic; ASTM D412
Flexural Modulus 0.0689 GPa
10.0 ksi
1% Secant; ASTM D790
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Compression Set 40 %
40 %
73°F, 70 hours; ASTM D395
71 %
71 %
158°F, 70 hours; ASTM D395
Processing Properties Metric English Comments
Middle Barrel Temperature 177 °C
350 °F
Front Barrel Temperature 182 °C
360 °F
Nozzle Temperature 191 °C
375 °F
Die Temperature 204 °C
400 °F
Melt Temperature 191 - 204 °C
375 - 400 °F