Polymer Property : Front Barrel Temperature = 329 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Front Barrel Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ F1005 Injection Molding Grade PHA Bioplastic
Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Front Barrel Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ F1006 Injection Molding Grade PHA Bioplastic
Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Front Barrel Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic
Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and ..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Huntsman AVALON® 70 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a speci..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and ..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
Front Barrel Temperature 165 - 190 °C
329 - 374 °F
Extrusion
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Front Barrel Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic
Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba..
Front Barrel Temperature 165 °C
329 °F
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic
Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom..