Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 154 - 171 °C | 310 - 340 °F | |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |