Processing Properties Metric English Comments
Front Barrel Temperature 154 - 171 °C
310 - 340 °F
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.