Material Notes:
Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offering an excellent long-term heat stability & productivity. This grade is used for: Connector, Pin of automobile, Power steering reservoir tank, Switch, Canister, Fuel filler tube. This product is available in Black color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 0.800 - 3.20 mm
V-2

@Thickness 0.0315 - 0.126 in
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 275 - 285 °C
527 - 545 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-275°C