Processing Properties Metric English Comments
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 242 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 246 - 266 °C
475 - 511 °F
A. Schulman ComAlloy Hiloy® 261 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 249 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 246 - 266 °C
475 - 511 °F
A. Schulman ComAlloy Hiloy® 262 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 246 - 266 °C
475 - 511 °F
A. Schulman ComAlloy Hiloy® 263 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.