Polymer Property : Middle Barrel Temperature = 455 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 235 °C
455 °F
For high temperature coextrusions.
DuPont Bynel® 21E553 Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG20 Flame Retardant, 20% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
Middle Barrel Temperature 235 - 280 °C
455 - 536 °F
Start Point: 260°C
Kingfa PC-S923 Modified PC
Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa UTPBT-HB Toughened PBT
Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
Injection Molding
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9..
Middle Barrel Temperature 235 - 245 °C
455 - 473 °F
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 420 Polyester - PBT, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 245 °C
455 - 473 °F
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin
30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)