Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 266 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Middle Barrel Temperature 254 - 266 °C
490 - 510 °F
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Middle Barrel Temperature 235 - 266 °C
455 - 510 °F
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S310
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA TW-17
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 249 - 266 °C
480 - 510 °F
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Middle Barrel Temperature 249 - 266 °C
480 - 510 °F
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized
Data provided by Clariant Masterbatches
Middle Barrel Temperature 249 - 266 °C
480 - 510 °F
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black
Data provided by Clariant Masterbatches
Middle Barrel Temperature 235 - 266 °C
455 - 510 °F
Diamond Polymers ABS/PC 8901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 260 - 266 °C
500 - 510 °F
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA TWP 502
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 246 - 266 °C
475 - 511 °F
A. Schulman ComAlloy Hiloy® 261 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 246 - 266 °C
475 - 511 °F
A. Schulman ComAlloy Hiloy® 262 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved