Polymer Property : Middle Barrel Temperature = 495 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 252 - 257 °C
485 - 495 °F
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced
Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex
Middle Barrel Temperature 246 - 257 °C
475 - 495 °F
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio..
Middle Barrel Temperature 238 - 257 °C
460 - 495 °F
Diamond Polymers ABS/PC FC-30
Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 238 - 257 °C
460 - 495 °F
Diamond Polymers ASA/PC FA-30
Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 241 - 257 °C
465 - 495 °F
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..