Polymer Property : Middle Barrel Temperature = 315 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 157 - 196 °C
315 - 385 °F
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **)
High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance..
Middle Barrel Temperature 157 - 207 °C
315 - 405 °F
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound  (discontinued **)
Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat..