Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance of 960 MPa making it extremely resistant to cracking and abuse. Parts made with IM62 are very resistant to harsh chemicals, solvents and to cleaning agents. IM62 offers flammability resistance. It is UL recognized: UL Std 94 V-0 and 5VA. It has excellent indoor UV color stability. It has good outdoor weatherability. It can be used for difficult parts. Passes FAR 25.853a.Processing: Drying is not typically required, however, if drying is needed dry at 55° for 4 hours. Barrel temperatures are typically 157 and196°C. Mold temperature should be between 32 and 60°C. Minimize the residence time in the barrel and keep melt temperatures between 196 and 207°C. To achieve a homogeneous melt, keep sufficient back pressure .7-2.8 N/mm^2. Before shutdown purge thoroughly and neutralize the mold. Contact Kleerdex Company for more information or refer to the Kydex Injection Molding Guide.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Melt Flow 34.2 g/10 min
34.2 g/10 min
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Flexural Yield Strength 67.0 MPa
9720 psi
ASTM D790
Flexural Modulus 2.245 GPa
325.6 ksi
ASTM D790
Izod Impact, Notched 9.60 J/cm

@Thickness 3.17 mm
18.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
annealed; ASTM D648
Flammability, UL94 5VA
5VA
V-0, UL Standard 94
Processing Properties Metric English Comments
Middle Barrel Temperature 157 - 196 °C
315 - 385 °F
Melt Temperature 196 - 207 °C
385 - 405 °F
Mold Temperature 32.2 - 60.0 °C
90.0 - 140 °F
Drying Temperature 54.4 °C
130 °F
Dry Time 4 hour
4 hour
Usually not needed