Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rate of heat release, and smoke generation.Features: Kydex IM90 is available in many standard and custom colors enabling you to satisfy both the functional and aesthetic requirements of any aircraft interior. Kydex IM90 is very resistant to a wide range of concentrated chemicals, and is therefore easy to clean with aggressive cleaners. Ammoniated cleaners should be avoided since they can leave a residue. Most importantly, Kydex IM90 meets the stringent requirements for the FAR 25.853 paragraph (d) in all thicknesses and colors. Radiant Panel: 2.41 as per ASTM E162Processing: Drying is not typically required, however, if drying is needed dry at 55° for 4 hours. Barrel temperatures are typically 157 and196°C. Mold temperature should be between 32 and 60°C. Minimize the residence time in the barrel and keep melt temperatures between 196 and 207°C. To achieve a homogeneous melt, keep sufficient back pressure .7-2.8 N/mm^2. Before shutdown purge thoroughly and neutralize the mold. Contact Kleerdex Company for more information or refer to the Kydex Injection Molding Guide.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 98 %
98 %
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 3.099 GPa
449.5 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.599 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 157 - 207 °C
315 - 405 °F
Melt Temperature 196 - 207 °C
385 - 405 °F
Mold Temperature 32.2 - 60.0 °C
90.0 - 140 °F
Drying Temperature 54.4 °C
130 °F
Dry Time 4 hour