PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPurge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Viscosity 105000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
105000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
10 sec; ASTM D2240
Tensile Strength at Break 12.2 MPa

@Temperature 23.0 °C
1770 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 220 %

@Temperature 23.0 °C
220 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 57.2 kN/m
326 pli
ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL 94
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 193 °C
360 - 379 °F
Middle Barrel Temperature 210 - 227 °C
410 - 441 °F
Front Barrel Temperature 227 - 238 °C
441 - 460 °F
Nozzle Temperature 227 - 238 °C
441 - 460 °F
Drying Temperature 70.0 °C
158 °F
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Descriptive Properties Value Comments
Agency Ratings UL 94 .QMFZ2.E76261
Appearance Black
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Slow-Moderate
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Connectors
Plugs
Wire & Cable Applications