Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 143 - 166 °C
290 - 330 °F
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.