Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 143 - 166 °C | 290 - 330 °F | |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |