Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 75.0 min @Temperature 4.00 °C |
1.25 hour @Temperature 39.2 °F |
Full Load |
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc.. |
|||
Cure Time | 75.0 min @Temperature 4.00 °C |
1.25 hour @Temperature 39.2 °F |
Full Load |
Chesterton MRS 5 Metal Rebuilding System MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we.. |
|||
Cure Time | 75.0 - 90.0 min @Temperature 121 °C |
1.25 - 1.50 hour @Temperature 250 °F |
|
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4.. |