Polymer Property : Cure Time = 1.25 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 75.0 min

@Temperature 4.00 °C
1.25 hour

@Temperature 39.2 °F
Full Load
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Cure Time 75.0 min

@Temperature 4.00 °C
1.25 hour

@Temperature 39.2 °F
Full Load
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..
Cure Time 75.0 - 90.0 min

@Temperature 121 °C
1.25 - 1.50 hour

@Temperature 250 °F
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4..