Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 30.0 - 40.2 min @Temperature 43.3 °C |
0.500 - 0.670 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b.. |
|||
Cure Time | 19.8 - 40.2 min @Temperature 43.3 °C |
0.330 - 0.670 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Cure Time | 19.8 - 40.2 min @Temperature 43.3 °C |
0.330 - 0.670 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Cure Time | 30.0 - 40.2 min @Temperature 82.2 °C |
0.500 - 0.670 hour @Temperature 180 °F |
De-mold Time |
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Cure Time | 30.0 - 40.2 min @Temperature 43.3 °C |
0.500 - 0.670 hour @Temperature 110 °F |
De-mold Time |
Northstar Polymers VEF-41 Viscoelastic Foam Formulation Viscoelastic foam has a very unique recovery property and very low compression deflection property. When the foam is compressed by a hand it can leave imprint of the hand, and then it slowly recove.. |
|||
Cure Time | 18.0 - 40.2 min @Temperature 80.0 - 100 °C |
0.300 - 0.670 hour @Temperature 176 - 212 °F |
|
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Cure Time | 30.0 - 40.2 min @Temperature 149 °C |
0.500 - 0.670 hour @Temperature 300 °F |
|
Master Bond FL901S Silver Filled, Electrically Conductive Adhesive Film Master Bond FL901S Polymer System is a high performance silver filled unsupported epoxy resin based adhesive film which offers outstanding performance characteristics and does not require refrigerat.. |