Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 0.670 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 30.0 - 40.2 min

@Temperature 43.3 °C
0.500 - 0.670 hour

@Temperature 110 °F
De-mold Time
Northstar Polymers FFM-1 Firm-Grade Flexible Open-Cell Foam
This foam formulation is particularly designed to make flexible but firm open-cell foam by either hand-mixing or machine casting. This material may be suitable for products that require some load b..
Cure Time 19.8 - 40.2 min

@Temperature 43.3 °C
0.330 - 0.670 hour

@Temperature 110 °F
De-mold Time
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and..
Cure Time 19.8 - 40.2 min

@Temperature 43.3 °C
0.330 - 0.670 hour

@Temperature 110 °F
De-mold Time
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at ..
Cure Time 30.0 - 40.2 min

@Temperature 82.2 °C
0.500 - 0.670 hour

@Temperature 180 °F
De-mold Time
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Cure Time 30.0 - 40.2 min

@Temperature 43.3 °C
0.500 - 0.670 hour

@Temperature 110 °F
De-mold Time
Northstar Polymers VEF-41 Viscoelastic Foam Formulation
Viscoelastic foam has a very unique recovery property and very low compression deflection property. When the foam is compressed by a hand it can leave imprint of the hand, and then it slowly recove..
Cure Time 18.0 - 40.2 min

@Temperature 80.0 - 100 °C
0.300 - 0.670 hour

@Temperature 176 - 212 °F
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Cure Time 30.0 - 40.2 min

@Temperature 149 °C
0.500 - 0.670 hour

@Temperature 300 °F
Master Bond FL901S Silver Filled, Electrically Conductive Adhesive Film
Master Bond FL901S Polymer System is a high performance silver filled unsupported epoxy resin based adhesive film which offers outstanding performance characteristics and does not require refrigerat..
Copyright © lookpolymers.com All Rights Reserved