Polymer Property : Cure Time = 30.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 1500 - 1800 min

@Temperature 22.0 °C
25.0 - 30.0 hour

@Temperature 71.6 °F
Dow Corning 3-4190 SILICONE GEL KIT
Two-part, transparent green, RT or heat cure, low viscosity, long shelf life.Information provided by Dow Corning
Cure Time 1440 - 1800 min

@Temperature 10.0 °C
24.0 - 30.0 hour

@Temperature 50.0 °F
De-Mold Time: 3.5-4 hrs
3M Scotchcast™ 2130 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it..
Cure Time 1440 - 1800 min

@Temperature 10.0 °C
24.0 - 30.0 hour

@Temperature 50.0 °F
De-Mold Time: 3.5-4 hrs
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu..