Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 35.000 - 40.000 min @Temperature 149 °C |
0.58333 - 0.66666 hour @Temperature 300 °F |
|
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Cure Time | 35.000 - 45.0 min @Temperature 149 °C |
0.58333 - 0.750 hour @Temperature 300 °F |
|
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen.. |