Polymer Property : Cure Time = 0.33333 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.016667 - 0.33333 min

@Temperature 24.0 °C
0.00027778 - 0.0055555 hour

@Temperature 75.2 °F
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..
Cure Time 0.0800 - 0.33333 min

@Temperature 24.0 °C
0.00133 - 0.0055555 hour

@Temperature 75.2 °F
BCC Products BC 100 Thin Cyanoacrylate Adhesive
BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas..