Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Cooling Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond.. |