Polymer Property : Screw Cooling Temperature = 158 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Cooling Temperature 50.0 - 70.0 °C
122 - 158 °F
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen
E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond..