Polymer Property : Zone 2 = 374 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® LW90-F2 POM, Tribological  (Unverified Data**)
Celcon® LW90-F2 is an acetal copolymer formulated with a nominal 9 melt flow rate base polymer and a standard level of polytetrafluoroethylene filler (PTFE). It is designed for use in wear applicat..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® AM90S POM, Specialty  (Unverified Data**)
Hostaform® acetal copolymer grade AM90S is a standard melt flow acetal copolymer grade containing an antimicrobial ingredient. Hostaform® AM90S provides the same physical and mechanical performan..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 2521 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusionInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 2521 G POM, Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusion, modified with (R) GUR (PE-UHMW)Information provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 36021 POM  (Unverified Data**)
Hostaform® C 36021 is an unfilled acetal copolymer grade formulated for high flow while retaining a good balance of mechanical properties.High flow, unfilled, for fast cycle & thin wallsInformation..
Zone 2 170 - 190 °C
338 - 374 °F
Extrusion Molding
LG Chemical KEYFLEX BT 10288D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 180 - 190 °C
356 - 374 °F
Injection Molding
Kolon ELLAS K-260D Thermoplastic Polyurethane
ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon.
Zone 2 175 - 190 °C
347 - 374 °F
Extrusion Molding
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Zone 2 180 - 190 °C
356 - 374 °F
Injection
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® M90SW POM, Tribological
Celcon M90SW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear against the same mating surface is important. This grade may be preferre..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 2521 LS POM, UV Resistant
Information provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 9021 K POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® MR130ACS POM, Specialty
Hostaform« acetal copolymer grade MR130ACS is a general purpose acetal with improved acid stabilization. Hostaform« MR130ACS demonstrates improved performance over standard acetals after intermit..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® S 27064 XAP POM, Impact Modified
Polyacetal copolymer, impact modifiedInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® S 27242 XAP² ™ POM, Impact Modified
Easy flow, impact modified injection molding grade, with good low temperature impact strength and good weld line strength and reduced emissions. Emission according to VDA 275 < 5 mg/kgInformation pr..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® SXT90Z-01 XAP POM, Impact Modified
Hostaform« acetal copolymer grade SXT90Z-01 XAP is UV stabilized, impact modified material available in a range of colors for automotive interior applications plus meets the typical low emission re..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® XGC25 POM, 25% Glass Reinforced
Hostaform« XGC25 is a Polyacetalcopolymer reinforced with approx. 25% glass fibres. Compared to the Hostaform« C 9021 GV 1/30 Hostaform« XGC25 has a higher strength.Information provided by Cel..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® XT 20 POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® M450 POM, Unfilled
Celcon« acetal copolymer grade M450 is an extremely low viscosity grade for optimal cycle performance in very thin walls or long, narrow flow paths in injection molding.Information provided by Cela..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® M90-34 POM, Unfilled
Celcon« M90-34 is a specially formulated injection moldable grade of acetal copolymer for the appliance market targeted at resisting staining while providing a balance of properties.Information pro..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® AM90S Plus POM, Specialty
Hostaform« acetal copolymer grade AM90S Plus is a standard melt viscosity acetal copolymer material containing an antimicrobial ingredient. AM90S Plus reaches maximum efficacy more rapidly than st..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 9021 M XAP²™ POM, Tribological
POM copolymerInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® XGC25-LW01 POM, 25% Glass Reinforced
Hostaform« XGC25-LW01 is an injection molding grade reinforced with approx. 25% glass fibers and tribological modification for sliding applications requiring low friction and wear.Information provi..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® GC10 POM, 10% Glass Reinforced  (Unverified Data**)
Celcon® GC10 acetal copolymer is a 10% glass reinforced acetal for improved strength and stiffness.10% glass fiber, has been replaced with Hostaform® C 9021 GV1/10Standard reciprocating screw inje..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® M25 POM  (Unverified Data**)
Celcon® acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Standard extrude..
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass fibersInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® S 27072 WS 10/1570 POM, Impact Modified  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POM-HIEasy flowing, elastomer-containing injection molding grade; black; weathering resistantInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® S 9243 XAP² ™ LS POM, Impact Modified  (Unverified Data**)
POM copolymer, modifiedImpact modified, UV stabilizedInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Zone 2 180 - 190 °C
356 - 374 °F
Celanese Celcon® MR270B POM, Specialty
Celcon« MR270B is a high flow specialty media resistant grade developed for improved bleach resistance.Information provided by Celanese