Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 245 - 255 °C | 473 - 491 °F | |
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 240 - 255 °C | 464 - 491 °F | Middle |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |