Polymer Property : Zone 2 = 491 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 245 - 255 °C
473 - 491 °F
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding
Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 255 °C
464 - 491 °F
Middle
BASF Nypel® 2351 HS BK PA6 (Dry)
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6..