Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Nypel® 2351 HS BK PA6 (Dry)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Nypel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Nypel® 2351 HS BK PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6 feedstocks. It possesses a balance of performance properties including low flex modulus and toughness. The heat stabilizer system extends its retention of properties at elevated temperatures.Application: Nypel® 2351 HS BK is generally recommended for applications such as convoluted and emission tubing, cable jacketing and other types of automotive tubing.Information provided by BASF
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
Nominal; ISO 527
Elongation at Yield 20 %
20 %
ISO 527
Tensile Modulus 1.20 GPa
174 ksi
ISO 527
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 0.920 GPa
133 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
ISO 180
13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ISO 75
Processing Properties Metric English Comments
Zone 1 230 - 250 °C
446 - 482 °F
Rear
Zone 2 240 - 255 °C
464 - 491 °F
Middle
Zone 3 230 - 250 °C
446 - 482 °F
Front
Zone 4 230 - 245 °C
446 - 473 °F
Head
Zone 5 230 - 245 °C
446 - 473 °F
Head
Die Temperature 230 - 245 °C
446 - 473 °F
Melt Temperature 250 - 260 °C
482 - 500 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.10 %
0.10 %
Descriptive Properties Value Comments
Color Black
Commercial Status North America