Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 205 - 215 °C | 401 - 419 °F | Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | |
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar. |