Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 205 °C | 401 °F | Injection |
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals Introduction: IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |
|||
Zone 1 | 205 - 220 °C | 401 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 205 °C | 401 °F | Compression Zone |
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Zone 1 | 205 °C | 401 °F | |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | Injection |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Zone 1 | 205 - 215 °C | 401 - 419 °F | |
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 205 - 315 °C | 401 - 599 °F | |
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 205 °C | 401 °F | Extrusion |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 1 | 205 °C | 401 °F | Feed zone |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Zone 1 | 205 °C | 401 °F | Feed zone |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Zone 1 | 205 °C | 401 °F | Feed zone |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Zone 1 | 205 °C | 401 °F | Feed zone |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Zone 1 | 205 °C | 401 °F | Injection |
Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance Introduction: IROGRAN A92K 4107 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |