Processing Properties Metric English Comments
Die Temperature 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Die Temperature 160 - 200 °C
320 - 392 °F
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Die Temperature 160 - 200 °C
320 - 392 °F
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Die Temperature 160 - 190 °C
320 - 374 °F
Extrusion Blow Molding
LG Chemical LUTENE-H BE0400 HDPE
Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con..
Die Temperature 160 - 170 °C
320 - 338 °F
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN ..
Die Temperature 160 - 180 °C
320 - 356 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 160 - 200 °C
320 - 392 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 160 - 180 °C
320 - 356 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 160 - 200 °C
320 - 392 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 160 - 180 °C
320 - 356 °F
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified  (discontinued **)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..