Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 179 °C | 355 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Die Temperature | >= 179 °C | >= 355 °F | |
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Borstar FR4803 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4803 offers a unique combination of good extrusion p.. |
|||
Die Temperature | 179 °C | 354 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Die Temperature | 179 °C | 355 °F | |
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Die Temperature | 179 °C | 355 °F | |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |