Polymer Property : Adapter Temperature = 379 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 193 °C
379 °F
5, Extrusion
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack..
Adapter Temperature 193 °C
379 °F
Extrusion
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and ..
Adapter Temperature 193 °C
379 °F
5, Extrusion
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Adapter Temperature 193 °C
379 °F
5, Extrusion
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el..
Adapter Temperature 193 °C
379 °F
5, Extrusion
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,..
Adapter Temperature 193 °C
379 °F
5, Extrusion
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..