Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 216 - 232 °C | 420 - 450 °F | |
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Adapter Temperature | 216 - 221 °C | 420 - 430 °F | |
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm.. |
|||
Adapter Temperature | 216 °C | 421 °F | 5, Extrusion |
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Adapter Temperature | 216 °C | 421 °F | 5, Extrusion |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Adapter Temperature | 216 - 232 °C | 421 - 450 °F | |
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,.. |