Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency and UV stability.Uses: Extrusion: Hose and Tube, Profile, Cable Jacket. Injection molding: Various.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore D 75

@Time 5.00 sec
75

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 40.7 MPa
5900 psi
ASTM D412
Elongation at Break 330 %
330 %
ASTM D412
100% Modulus 0.0220 GPa
3.19 ksi
ASTM D412
300% Modulus 0.0270 GPa
3.92 ksi
ASTM D412
Tear Strength 26.3 kN/m
150 pli
Trouser; ASTM D470
Graves Tear Strength 245 kN/m
1400 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 68

@Load 1.00 kg
68

@Load 2.20 lb
H-18 wheel; ASTM D3389
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
DSC
Glass Transition Temp, Tg -10.0 °C
14.0 °F
DSC
Processing Properties Metric English Comments
Zone 1 204 °C
399 °F
Extrusion
Zone 2 210 °C
410 °F
Extrusion
Zone 3 216 °C
421 °F
Extrusion
Zone 4 216 °C
421 °F
Extrusion
Adapter Temperature 216 °C
421 °F
5, Extrusion
Die Temperature 218 °C
424 °F
6, Zone 1, Extrusion
218 °C
424 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Users viewing this material also viewed the following: