Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 216 - 232 °C | 420 - 450 °F | |
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Adapter Temperature | 216 - 221 °C | 420 - 430 °F | |
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm.. |