Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 182 - 193 °C | 360 - 379 °F | Extrusion |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |