Polymer Property : Adapter Temperature = 360 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 182 °C
360 °F
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
ApplicationsAQUATHENE FR 4098-00 is a colorable flame retardant masterbatch designed specifically for moisture cure applications. When FR 4098-00 is combined with AQ 120-000 and CM 04482 in the cor..
Adapter Temperature 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio..
Adapter Temperature 182 °C
360 °F
5, Extrusion
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast..
Adapter Temperature 182 - 193 °C
360 - 379 °F
Extrusion
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..
Adapter Temperature 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane
Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur..