Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cycle Time - Injection = 35 sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cycle Time - Injection 35 - 45 sec
35 - 45 sec
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Cycle Time - Injection 35 - 45 sec
35 - 45 sec
Lubrizol Estane® T465A Thermoplastic Polyurethane
Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M104N MPPO Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M105N MPPO Resin
High flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M106 MPPO Resin
Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M104 MPPO Resin
Flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Cycle Time - Injection 35 sec
35 sec
Beijing Chemical Industry KAIFA® M106N MPPO Resin
High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)